TECHNET Archives

August 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 25 Aug 1999 22:06:11 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Enter your name here <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Enter your name here <[log in to unmask]>
Parts/Attachments:
text/plain (70 lines)
One of the reasons, years ago, we all attempted to run as fast as possible
away from DFSM is it doesn't adhere well to much of anything.

Earl Moon
----- Original Message -----
From: Stephen R. Gregory <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, August 25, 1999 2:27 PM
Subject: [TN] Dry Film Soldermask Adhesion..


> Hi Ya'll!
>
> I've had one of our buyers come to me with a problem that we have with one
of
> the fabs we buy.
> I'm no expert on fabs by a long shot, but I told him know where to ask (am
I
> kissing-up enough? Hehehe...)
>
> Problem is with a fab (GFG laminate) that our customer is specifying dry
> film...they want to ensure the via's
> are tented. There isn't a brand specified, but they do want the fab masked
in
> accordance with IPC-SM-840 Class-3
> Type B dry film. Our fab vendor has chosen to use a Dynachem dry film. The
> problem we're having is that the mask is
> flaking from the bare copper. The fab vendor is suggesting that our
cleaning
> chemistry may be causing the problem.
> We're using Aquanox XJN in a MCS-1000 Electrovert cleaner. The wash
> temperature is 140 F., and my rinse is 120 F.
>
> Know what might be causing this? Do you recommend any other brand dry
film?
>
> Thanks!
>
> -Steve Gregory-
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2