Larry,
The call out is for base material and refers to:
"G"- glass fabric woven,
"E"- non flame resistant epoxy,
"062"- .062" thick,
"C"- drum side out electrodeposited copper foil,
"2/2"- double sided laminate with 2 oz. copper per square
foot on each side.
The call out comes from the old MIL-P-13949 base material specs. The
current MIL spec is MIL-S-13949H and there is an IPC version, which I
believe is still in the "Interim Final" circulation, IPC-4101.
Hope this helps.
Keith Larson
North Texas Circuit Board
At 09:06 AM 8/27/97 -0600, you wrote:
>Hello:
>
>I have an old drawing that calls out FL-GE062C2/2.
>
>Can someone tell me what this is calling out and what Mil-Spec it is
>refering to?
>
>Thanks;
>
>Larry L. Pucket
>Senior PCB Layout Designer
>Sandia National Laboratories
>P.O. Box 5800 MS-0624
>Albuquerque, NM 87185-0624
>
>Phone: (505)844-1711
> Fax: (505)844-7428
>
>Email: [log in to unmask]
>
>
|
|
|