Gentlemen I have a new technology water borne CONFORMAL coating for printed
circuit boards. Any suggestions as to how I can take this to market. In
addition to a clear with detectable dye, I have a black CONFORMAL coating to
conceal components. Also have an organic dissolver for acrylic, urethane and
silicon coatings.

Please contact Jim Fraser at 440-729-0450 or fax 440-729-0484 or via email
[log in to unmask]