TECHNET Archives

April 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Bev Christian <[log in to unmask]>
Date:
Tue, 2 Apr 2002 18:40:04 -0500
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Bev Christian <[log in to unmask]>
Parts/Attachments:
text/plain (27 lines)
Technetters,
To a certain extent I am aware of the work the NEMI tin whisker task force
and various connector/component manufacturers are doing about 100% tin
coatings.  But I am still left with several questions whose answers I have
missed or questions that have not been addressed.  So... here goes - the
immersion tin coating are for SMT pads that are going to be soldered.  What
are people doing about test points? Are there stencil openings to put solder
on these pads as well?  Or are these pads left unsoldered?  Has anyone
carried out any testing with regards to the tendency of these materials to
grow/not grow whiskers? Or do the organics in the coating completely kill
that possibility?

regards,
Bev Christian
Research in Motion

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2