Ingemar, and others:
While we're on the subject:
We also use 'stoneage' technique to inspect nickle/gold
plating from sub-contractor. He's using some sort of
non-destructive method to verify thickness, and we do not
always agree on the result.
Apart from the obvious problem of thichness variation over
the panel, is there a predictable difference in thickness
found using different techniques?
Regards
Torben Østeraa
Printca AS
Denmark
>>-----Original Message-----
>>From: Ingemar Hernefjord (EMW)
>>[mailto:[log in to unmask]]
>>Sent: Tuesday, October 05, 1999 8:42 AM
>>To: [log in to unmask]
>>Subject: Re: [TN] Measurements of Gold over Nickel
>>
>>
>>Edward,
>>we have found that there is nothing better than ordinary
>>stoneaged crossectioning and study in a metalographic
>>microscope. In mass production, samples are usually enough.
>>Such examinations don't take time and they tell a lot more
>>than betascope. And...you can store the images and have a
>>look back up and then.
>>Regards
>>Ingemar Hernefjord
>>Ericsson Microwave Systems
>>
>>
>>I am looking after alternative method of measuring of
>>electroplated Gold
>>over Nickel for production .Gold thickness is in range from
>>0.75 to 2.5
>>microns.
>>I have in my plant beta scope with Promethium source with lot
>>of problems.I
>>have also XRF,that can not be placed in production area.
>>Any sugestions?
>>
>>Edward Szpruch
>>Eltek , Manager of Process Engineering
>>P.O.Box 159 ; 49101 Petah Tikva Israel
>>Tel ++972 3 9395050 , Fax ++972 3 9309581
>>e-mail [log in to unmask]
>>
>>##############################################################
>>TechNet Mail List provided as a free service by IPC using
>>LISTSERV 1.8c
>>##############################################################
>>To subscribe/unsubscribe, send a message to [log in to unmask]
>>with following text in
>>the body:
>>To subscribe: SUBSCRIBE TECHNET <your full name>
>>To unsubscribe: SIGNOFF TECHNET
>>##############################################################
>>Please visit IPC web site (http://www.ipc.org/html/forum.htm)
>>for additional
>>information.
>>If you need assistance - contact Gayatri Sardeshpande at
>>[log in to unmask] or
>>847-509-9700 ext.5365
>>##############################################################
>>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|