We have had a Fischerscope XRF in the plating environment, namely
right next to our nickel gold platig line for nearly 13 years without
any malfunctions due to the environment. We have found it to be +/-
10% accurate on gold thickness from 5-200 microinches. However, the
nickel measurement accuracy and precision drops off rapidly if the
gold thickness is over 90 microinches. Although you can measure
nickel/gold metallurgically, the gold thickness, which is usually 50
microinches or less in our applications, is very difficult to measure
unless you have greater than 1000x magnification. Nickel can be
measured metallurgically, but takes much longer and more resources
than XRF.
Michael Holan
HADCO Corp.
Austin, TX
512-246-5612
______________________________ Reply Separator _________________________________
Subject: [TN] Measurements of Gold over Nickel
Author: edward edward szpruch <[log in to unmask]> at smtplink-hadco
Date: 10/5/99 8:34 AM
I am looking after alternative method of measuring of electroplated Gold
over Nickel for production .Gold thickness is in range from 0.75 to 2.5
microns.
I have in my plant beta scope with Promethium source with lot of problems.I
have also XRF,that can not be placed in production area.
Any sugestions?
Edward Szpruch
Eltek , Manager of Process Engineering
P.O.Box 159 ; 49101 Petah Tikva Israel
Tel ++972 3 9395050 , Fax ++972 3 9309581
e-mail [log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|