TECHNET Archives

February 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Reply To:
Date:
Wed, 05 Feb 1997 22:15:36 +0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (32 lines)
Scott B. Westheimer wrote:
> 
> From: Scott Westheimer
> Date: 2/5/97
> 
> Have anyone heard of a new oxide treatment or reducer from Japan called MEC
> etch bond? Any information would be appreciated.
Dear sir,
If you need the oxide treatment process based on horizontal
system,dark-brown color,no-pink ring...
I suggest you can contact Alpha-Metals.
The process is "Alpha-Prep" only two - three stages.
1 cleaner ------ dwell time 30 -40 sec 40 drgree C 
2.pre dip  ----- dwell time 10 sec     RT
3.alpha-prep --- dwell time 30 sec     35 drgree C 

B Regs
Carl E. Chiang
Project Manager

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2