Scott B. Westheimer wrote: > > From: Scott Westheimer > Date: 2/5/97 > > Have anyone heard of a new oxide treatment or reducer from Japan called MEC > etch bond? Any information would be appreciated. Dear sir, If you need the oxide treatment process based on horizontal system,dark-brown color,no-pink ring... I suggest you can contact Alpha-Metals. The process is "Alpha-Prep" only two - three stages. 1 cleaner ------ dwell time 30 -40 sec 40 drgree C 2.pre dip ----- dwell time 10 sec RT 3.alpha-prep --- dwell time 30 sec 35 drgree C B Regs Carl E. Chiang Project Manager *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************