Ed Popielarski <[log in to unmask]>
Date:
Fri, 8 Aug 2014 12:32:24 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Subject:
From:
Steve Gregory <[log in to unmask]>
X-cc:
TechNet E-Mail Forum <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (183 lines)
Yeah Ed, that was my first idea, but we don't have any here small enough
diameter to fit in the footprint. I think we're just going to hand solder
them in...

Steve


On Fri, Aug 8, 2014 at 10:29 AM, Ed Popielarski <[log in to unmask]>
wrote:

>  Dissopads
>
>
>
>
>
>
>
> Ed Popielarski
>
> Engineering Manager
>
>
>
>                                 970 NE 21st Ct.
>
>                               Oak Harbor, Wa. 98277
>
>
>
>                               Ph: 360-675-1322
>
>                               Fx: 206-624-0695
>
>                               Cl: 949-581-6601
>
>
>
>        “It's one kind of victory to slay a beast, move a mountain, and
> cross a chasm, but it's another kind altogether to realize that the beast,
> the mountain, and the chasm were of your own design.”
>
>
> https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
>
>
>
> *From:* Steve Gregory [mailto:[log in to unmask]]
> *Sent:* Friday, August 08, 2014 8:59 AM
> *To:* Ed Popielarski
> *Cc:* TechNet E-Mail Forum
> *Subject:* Re: [TN] Unusual part thingy....
>
>
>
> Hi again all!
>
>
>
> Well, I have learned something this morning! But I learned something else
> too, this little jewel will have to be stood up a little somehow because
> the footprint is such that it will drop down flush to the board and then
> have a possibility of the case shorting to the pads:
>
>
>
> http://stevezeva.homestead.com/SD211DE_Footprint.jpg
>
>
>
> There's no insulator called out in the BOM, and worse yet, these parts
> have already been prepped without taking into account a stand-off height
> for the part......(heavy sigh). Well I suppose if there wasn't problems, I
> wouldn't have a job.....('nuther heavy sigh)
>
>
>
> Steve
>
>
>
> On Fri, Aug 8, 2014 at 9:23 AM, Ed Popielarski <[log in to unmask]>
> wrote:
>
> Old school ESD protection. We're talking about '70s stuff here. Remove it
> in an ESD protected environment and throw it away. It's a dead short
> between leads and should not be soldered in place.
>
> Ed Popielarski
> Engineering Manager
>
>
>                                970 NE 21st Ct.
>                               Oak Harbor, Wa. 98277
>
>                               Ph: 360-675-1322
>                               Fx: 206-624-0695
>                               Cl: 949-581-6601
>
>        “It's one kind of victory to slay a beast, move a mountain, and
> cross a chasm, but it's another kind altogether to realize that the beast,
> the mountain, and the chasm were of your own design.”
>
> https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
> Sent: Friday, August 08, 2014 8:08 AM
> To: [log in to unmask]
> Subject: [TN] Unusual part thingy....
>
> Morning All,
>
> One of my inspectors was doing a first article inspection on a board and
> came to me with a question about a transistor that is on the board, it's
> this one here:
>
>
> http://www.futureelectronics.com/en/technologies/semiconductors/discretes/transistors/mosfets/Pages/3792082-SD211DE.aspx?IM=0
>
> She was asking me what this little wire thingy is on the leads of the
> part, I said I didn't know...I have never seen something like this before.
> I'm thinking that it may be some sort of stand-off that you slide up and
> down the leads depending on how high you want the part to be stood up off
> the board, but I'm not sure. The datasheet doesn't say anything about it,
> and like I said, this is the first time I've seen this (okay, I've lead a
> sheltered life...   ;^)  )
>
> So what is this thingy?
>
> http://stevezeva.homestead.com/SD211DE.jpg
>
> Steve
>
> --
>
>
> This email and any attachments are only for use by the intended
> recipient(s) and may contain legally privileged, confidential, proprietary
> or otherwise private information. Any unauthorized use, reproduction,
> dissemination, distribution or other disclosure of the contents of this
> e-mail or its attachments is strictly prohibited. If you have received this
> email in error, please notify the sender immediately and delete the
> original.
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
>
>
>
>
>
>
> This email and any attachments are only for use by the intended
> recipient(s) and may contain legally privileged, confidential, proprietary
> or otherwise private information. Any unauthorized use, reproduction,
> dissemination, distribution or other disclosure of the contents of this
> e-mail or its attachments is strictly prohibited. If you have received this
> email in error, please notify the sender immediately and delete the
> original.
>

-- 


This email and any attachments are only for use by the intended 
recipient(s) and may contain legally privileged, confidential, proprietary 
or otherwise private information. Any unauthorized use, reproduction, 
dissemination, distribution or other disclosure of the contents of this 
e-mail or its attachments is strictly prohibited. If you have received this 
email in error, please notify the sender immediately and delete the 
original. 

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.