TECHNET Archives

April 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Graham Savage <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 22 Apr 1998 11:01:59 +0930
Content-Type:
text/plain
Parts/Attachments:
text/plain (34 lines)
Copper/Aluminium clad Teflon Plating

Specifically, my query concerns plating 0.5oz to 1oz copper on Teflon
with 1/8 to 1/4 Aluminium back (6061).

What is the best method of activating the Aluminium surface prior to
plating without using a nitric desmut, as this attacks the copper
surface.
or
What can be used for removing the smut on the Aluminium surface after
etching in a potassium fluoride etch which will not attack the copper
surface.

How can I achieve maximum adhesion of electroless nickel on Aluminium,
such as double dipping in Zincate. without stripping the Zincate with
Nitric

Thanks in advance

Graham Savage
[log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2