Hi Ioan:
You would definitely need a drain at the
bottom of the box. Humidity will condense inside and will accumulate
over time, if it can get inside. Dendrites will form if there are salts
left from poor cleaning of flux. Conformal Coating diminishes the
dendrite growth.
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: Tuesday, November 29, 2005 11:44 AM
To: [log in to unmask]
Subject: [TN] Humidity and enclosed RF board
Hi Technos,
application: one RF board and one antenna, no conformal coating, both
sealed inside of a casing; outdoor unit, will see temp and humidity
variations.
question: assuming that the boards are well insulated from the exterior,
should I worry about long term rel of the boards? Otherwise said, due to
temp variations, can the residual humidity inside the casing condensate
on the boards and cause damage? Or can it make grow dendrites?
And a general question: For dendrites we need a potential difference,
humidity and dirt; is there any threshold for the humidity level, below
which dendrites will not grow?
Thank you,
Ioan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|