Hi Ioan: You would definitely need a drain at the bottom of the box. Humidity will condense inside and will accumulate over time, if it can get inside. Dendrites will form if there are salts left from poor cleaning of flux. Conformal Coating diminishes the dendrite growth. Regards, Ramon -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan Sent: Tuesday, November 29, 2005 11:44 AM To: [log in to unmask] Subject: [TN] Humidity and enclosed RF board Hi Technos, application: one RF board and one antenna, no conformal coating, both sealed inside of a casing; outdoor unit, will see temp and humidity variations. question: assuming that the boards are well insulated from the exterior, should I worry about long term rel of the boards? Otherwise said, due to temp variations, can the residual humidity inside the casing condensate on the boards and cause damage? Or can it make grow dendrites? And a general question: For dendrites we need a potential difference, humidity and dirt; is there any threshold for the humidity level, below which dendrites will not grow? Thank you, Ioan --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------