TECHNET Archives

August 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 9 Aug 2005 12:51:31 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Peter Swanson <[log in to unmask]>
Subject:
From:
Peter Swanson <[log in to unmask]>
X-cc:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (65 lines)
Since the demise of 1,1,3-based cleaning systems and a general move to
no-clean processing, I believe that there are few (if any) temporary
masks still commercially available which are removable with defluxing
solvents... unless you include water as a solvent (which it is, of
course!). This process if often done with water soluble temporary
masking materials, of which there are a number available.

Regards, 
Peter 
--
--------------------------------------------------------
Peter Swanson           [log in to unmask]
INTERTRONICS               http://www.intertronics.co.uk
Tel: +44 1865 842842                Oxfordshire, England
INTERTRONICS is dedicated to providing quality material, 
consumable and equipment solutions to the high 
technology, high performance assembly industries, 
incorporating outstanding levels of technical support 
and customer service.

Read our blog! http://www.intertronics.co.uk/blog/blog.htm

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: 08 August 2005 18:24
To: [log in to unmask]
Subject: Re: [TN] Cleaning of gold wirebond pads

Gold pads/fingers can be easily protected & cleaned by applying a
solvent soluble maskant to the parts, then removing when ready with a
suitable  solvent.
See NEPCON West Proceedings, 1981- the details are in a paper by G. J.
Engelland.

Bill  Kenyon
Global Centre Consulting
3336 Birmingham Drive
Fort Collins, CO  80526
Tel: 970.207.9586 Cell: 970.980.6373
email:  [log in to unmask]


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2