Hi Grant! Components which use either a AgPd or a AgPdPt termination
finish can be problematic at times. Both of these termination finishes
tend to have short shelf lives in terms of solderability. It is not
uncommon to only have a 3-6 month solderability shelf life - in comparison
to many component finishes which have a 12 month solderability shelf life.
Also, many of the components with a AgPd or a AgPdPt termination finish
have a solder-ability concern of leaching the termination finish off the
component resulting in a loss of solder joint integrity. I wouldn't
necessarily say that the a AgPd or a AgPdPt termination finishes are not
compatible with a Pbfree soldering process but the higher process
temperatures of SAC soldering processes is going to accelerate the
leaching of the termination finish so you will have a significantly
reduced process window in comparison to a tin/lead process. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Grant Emandien <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
07/02/2008 04:19 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Grant Emandien <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Silver-Palladium termination SMT solder problems
Hi all,
We are experiencing poor solderability with AgPd-terminations on MOVs
exposed to a lead-free reflow profile using a SAC alloy on an
ENIG-finished PCB. Though we have run this board only once previously
with the same part finish using a lead-rich alloy, we had similar
effects but not to the extent we are now experiencing.
Can anyone provide some insight into this/
Regards
Grant
**********************************************************************
Relevant company disclaimers are available at the following addresses:
Tellumat (Pty) Ltd e-mail:
mailto:[log in to unmask]
Web: http://www.tellumat.com/email.aspx
**********************************************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|