TECHNET Archives

May 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Jorge Engenharia <[log in to unmask]>
Date:
Wed, 12 May 1999 08:59:48 -0400
Content-Type:
text/plain
MIME-Version:
1.0
Reply-To:
"\"TechNet E-Mail Forum.\" <[log in to unmask]>, Jorge Engenharia" <[log in to unmask]>
Parts/Attachments:
text/plain (84 lines)
  Hi;

  Today I find a catalog from a local representative of ERSA company, they
have a wave soldering machine named SO-NO-CLEAN that is fluxless and using
ultrasonics into the solder wave ( 20 KHz ) inside a sealed n2 chamber. So
the ability to make hundreds of solder joints is now available. The strange
thing is their web site don`t mention anything about that ...
http://www.ersa.de/emach_e.htm

 Jorge Dourado de Santana
Maintenance / Process Engr
Microtec - Brazil



> -----Original Message-----
> From: [log in to unmask] [SMTP:[log in to unmask]]
> Sent: 8 de Maio de 1999 06:35
> To:   [log in to unmask]
> Subject:      Re: [TN] (Fwd) Ultrasonic soldering
>
> In a message dated 07/05/99  07:28:01AM,  [log in to unmask]
> writes:
>
> My cynical two penneth:
> Interesting articles appear every few years putting forward ultrasonic
> soldering....
> but it never seems to go anywhere.
> Less cynically:
> I think possibly this is not because it doesn't work, but because it does
> away with the main advantage of the soldering process which is its ability
> to
> make hundreds of joints similtaneously. Where u/s is used industrially for
> joining it seems to be in welding where joints are made individually,
> these
> range from applications like wirebonding to joining plastics.
>
> Mike Fenner
> ..............
> > Hello all,
> >
> >  I have just been reading an article on Ultrasonic soldering
> >  which looks interesting, has anyone out there had had any
> >  experience of this process?
> >
> >  Thanks,
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2