Steve is right. These residues are conductive, moisture absorbing and will
cause electrical leakage problems in the field. Just place a unit on
functional test in a hot dry room and watch it pass, then take the unit place
it in a humidity chamber at 35C 65%RH overnight (16 hours) then retest the
unit (use proper safety precautions).
Terry Munson
<< YAAAAAAAAAAAAAAAHHHHHHHHHH!!!!!!!!!!
BE HORRIFIED!!!!! STOP!!! STOP!!!! STOP!!!!! (pant, pant, pant....)
Just because it looks better to pass QA visual inspection, doesn't mean
squat...runs these boards through SIR testing and you'll probably have a
heart attack!!
The big question I have, is why in the world is your customer requiring you
not to clean after rework? Seems kinda' senseless if you ask me...
By ALL MEANS, STOP THIS PRACTICE NOW!!!!!!!!!!
>>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|