Does this make you happier?
http://www.ngk.co.jp/english/MTL/products/bery/008/0005/main.html
Inge
----- Original Message -----
From: "Roberts, Jon" <[log in to unmask]>
To: "TechNet E-Mail Forum" <[log in to unmask]>; "Inge"
<[log in to unmask]>
Sent: Tuesday, October 07, 2008 9:08 AM
Subject: RE: [TN] SOLDERING BERYLLIUM COPPER
To clarify, we are purchasing this contact for use on a Mac Panel
connector and the contact is designed to be crimp. No where does the
datasheet indicate you can solder. Engineering is trying to solder since
the wire gage does not match the contact size. It is on a test set.
Thanks, Jon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
Sent: Tuesday, October 07, 2008 10:57 AM
To: [log in to unmask]
Subject: Re: [TN] SOLDERING BERYLLIUM COPPER
The Copper is just 'doped' with Be, still solderable. We have soldered
to
BeCu without any problems. The thing is you must polish or burnish the
metal
and solder asap. Barrier layer, well it depends..(Dough TM). Remember
that
billions of solder joints have survived for a century in old radios etc.
They hardly knew what a barrier was at that time. Soldering to Nickel is
not
my favorite. IF you must declare a present barrier, avoid bright hard
Nickel. Matte sulfamate is better.
Inge
----- Original Message -----
From: "Roberts, Jon" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, October 07, 2008 7:47 AM
Subject: [TN] SOLDERING BERYLLIUM COPPER
Is there any issue with soldering a crimp style contact that is
beryllium copper with gold finish? I am used to having nickel barrier
over the base material. Internet search does find you can but it
indicates it is not a strong connection. Thanks, Jon
This communication is intended only for use by the addressee(s) named
herein
and may contain business confidential and/or legally privileged
information.
If you are not the intended recipient of this e-mail, you are hereby
notified that any dissemination, distribution, disclosure or copying of
this
e-mail and its contents is strictly prohibited. If you have received
this
e-mail in error, kindly notify the sender by replying to this message.
In
addition, please permanently delete the message and any attachments
without
copying or disclosing the contents. Thank you for your cooperation.
THIS DOCUMENT AND/OR SHIPMENT MAY CONTAIN COMMODITY ITEMS, SOFTWARE OR
TECHNICAL DATA THAT IS CONTROLLED BY U.S. EXPORT LAW, AND MAY NOT BE
EXPORTED OUTSIDE THE UNITED STATES OR TO NON U.S. PERSONS WITHOUT THE
APPROPRIATE EXPORT LICENSE FROM EITHER THE U.S. DEPARTMENT OF STATE OR
DEPARTMENT OF COMMERCE.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
This communication is intended only for use by the addressee(s) named herein
and may contain business confidential and/or legally privileged information.
If you are not the intended recipient of this e-mail, you are hereby
notified that any dissemination, distribution, disclosure or copying of this
e-mail and its contents is strictly prohibited. If you have received this
e-mail in error, kindly notify the sender by replying to this message. In
addition, please permanently delete the message and any attachments without
copying or disclosing the contents. Thank you for your cooperation.
THIS DOCUMENT AND/OR SHIPMENT MAY CONTAIN COMMODITY ITEMS, SOFTWARE OR
TECHNICAL DATA THAT IS CONTROLLED BY U.S. EXPORT LAW, AND MAY NOT BE
EXPORTED OUTSIDE THE UNITED STATES OR TO NON U.S. PERSONS WITHOUT THE
APPROPRIATE EXPORT LICENSE FROM EITHER THE U.S. DEPARTMENT OF STATE OR
DEPARTMENT OF COMMERCE.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|