Siggi,
I know that TI generated a BGA Solderability Test method, based on the
technique described in EIA/JESD22-B102C, Solderability Test Method. They
used a reflow soldering oven to perform the test and a blank ceramic card.
You can get a description of the test method from TI's website.
I tried it with a SMT rework station, using a glass slide. I found that you
could achieve the same type of results with the rework station as with the
reflow oven and ceramic card.
Give me a call off line some time. Hope this helps.
Good Luck.
Lee Whiteman
Senior Manufacturing Engineer
E-Mail: [log in to unmask] <mailto:[log in to unmask]>
Ph: (610) 362-1200 x208
Fax: (610) 362-1290
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Zweigart, Siegmund
> Sent: Thursday, March 14, 2002 4:03 AM
> To: [log in to unmask]
> Subject: [TN] Solderability of BGA
>
>
> Hello
>
> I am looking for some documents about solderability tests for BGA s with
> eutectik balls. Can anybody help me in this subject?
> We think that the BGA- Balls were touched by fingers and the
> solderiability
> is significant reduced.
> How can we analyse the component for fingerprints? We are thinking of
> looking for NaCl.
> Has anybody another idea?
>
> Siggi
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources &
> Databases > E-mail Archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|