TECHNET Archives

November 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Eric Dawson <[log in to unmask]>
Date:
Mon, 12 Nov 2001 13:49:56 -0000
Content-Type:
text/plain
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (46 lines)
Hi All,

I notice that a few new references have been made to the above subject and
thought I would share some of my early work with you.

In my first post as a graduate, I researched the causes of dewetting on
circuit boards. I came across a solution, the make-up of which I have since
lost, which dissolved the tin lead alloy but left the two intermetallic
layers.

I produced a number of one inch square coupons which I soldered using 63/37
alloy, RMA flux and a Tri Moore Rotary Dip Tester.

These were divided into three categories:

1       Control
2       Remove tin lead and re test in the Rotary Dip.
3       Remove tin lead, Several hours steam ageing and re test.

Microsections showed that I had taken off the alloy successfully and left
the IMC.s.

All of the re tested coupons soldered successfully, including the steam aged
ones.

This was some years ago so I cannot remember the etchant nor the hours and
conditions in the steam ageing equipment. I do remember that the IMC
soldered very well so I am always dubious when somebody blames the
intermetallic for poor soldering.

I seem to be alone in my faith that the IMC solders but this was the result
of my very own work and I stand by it.

Regards
Eric Dawson, Defender of the IMC.

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2