TECHNET Archives

November 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Eric Dawson <[log in to unmask]>
Date:
Mon, 19 Nov 2001 08:20:31 -0000
Content-Type:
text/plain
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (59 lines)
Hi Tom,
Are you wave soldering the other side of the board with the reflow soldered
bga.s on top? I have come across this practice and it definitely disturbs
the bga joints causing opens which cannot be detected by ordinary X ray
inspection.
Hope this helps.
Regards
Eric Dawson

> -----Original Message-----
> From: Tom Colby [SMTP:[log in to unmask]]
> Sent: Friday, November 16, 2001 8:47 PM
> To:   [log in to unmask]
> Subject:      [TN] BGA bone of contention
>
> Help me out with this technetters,
>
> The problem: BGA opens on a HASL board.
>
> The device: Motorola MCF5272, a 196 MAPBGA, 1mm pitch, ball size of
> 0.35/0.65. Substrate land size unknown. Footprint designed with a pad  of
> 0.28mm.
>
> Management's solution is to increase the pad size to 0.4mm. I say to look
> elsewhere in the process for the problem.
>
> I'd like to hear the opinions of my esteemed colleagues. What do you say
> folks?
>
> Thanks in advance,
>
> Tom
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2