Dan,
This brings up an interesting point. We tend to run large amounts of current through our lugs. (Oh, brain cramp - we can't run more current through the lug than the wire can handle, duh! Talk about needing coffee, geeze!) I'll use this as an argument with my engineers who insist on soldering all crimped lugs due the "lots of current" they are running through the connection. I guess we are trapped in the "we've always done it this way" syndrome.
To add onto Kathy's point, if we were to use RA or RMA flux solder for wires, how do I keep my assemblers from using the OA flux solder we use for circuit boards?
Phil Nutting
-----Original Message-----
From: Dan R. Johnson [mailto:[log in to unmask]]
Sent: Thursday, May 16, 2002 11:01 AM
To: [log in to unmask]
Subject: Re: [TN] Crimped connections
Good Morning Stu,
Two good reasons *not* to solder crimped connections.
1) it defeats the natural strain relief built into a crimped connection.
2) it introduces flux into the connection that cannot be removed since it
wicks past the insulation.
3) the connectors are designed not to be used with solder. (OK I don't count
so good, where's the coffee?)
Dan
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|