When you mix high purity "low drossing" solders that contain Ph with lower
purity solders you will create more dross than with either of the two when used
seperately.  I don't see a problem when mixing two lower grades...but the
mixture can be catostrophic to a wave solder machine.  The nature of the organic
low drossing additives pull contaminates out and to the top.  I would just
understand my chemistries before mixing them up.



[log in to unmask] on 07/28/99 04:51:43 PM

Please respond to [log in to unmask]; Please respond to
      [log in to unmask]

To:   [log in to unmask]
cc:    (bcc: Jason Smith/Lex/Lexmark)
Subject:  Re: [TN] Mixing solder bars from different manufacturer's




Jim,
Ah there's the rub, in your last phrase - "if any quality issues could
arise".  If it were to happen, for whatever reason, each solder bar
manufacturer could then point at the other.  Unless you are talking a lot of
solder I would recycle it or use it in a small static solder pot, not in one
of your wave solder machines.

regards,
Bev Christian
Nortel Networks

> -----Original Message-----
> From: West, Jim [SMTP:[log in to unmask]]
> Sent: Wednesday, July 28, 1999 4:40 PM
> To:   [log in to unmask]
> Subject:      [TN] Mixing solder bars from different manufacturer's
>
> Hi all,
>
> This might be a silly question, but I received some left over solder from
> a
> customer that is made by a different manufacturer than what we use.  Both
> solder bars are 63/37 and I want to know if you can mix solder from
> different manufacturers, I'm not sure if manufacturers do anything
> different
> with their product or if any quality issues could arise.
>
> Thanks,
>
>
> Jim West
> Manufacturing Engineer
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2