TECHNET Archives

April 2016

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
David Hillman <[log in to unmask]>
Date:
Fri, 8 Apr 2016 10:44:51 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Message-ID:
Subject:
From:
Steve Gregory <[log in to unmask]>
X-cc:
TechNet E-Mail Forum <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (106 lines)
Hi again Dave,

So the PCB is a .090" thick, 8-layer board, the stack-up is this:

Soldermask
Layer 1
----------
Ground
----------Pre-preg
Layer 3
----------
+12V
----------Pre-preg
-12V
----------
Layer 6
----------Pre-preg
Ground
----------
Layer 8
Soldermask

Steve


On Fri, Apr 8, 2016 at 10:18 AM, David Hillman <
[log in to unmask]> wrote:

> Hi Steve - yes, you have enough physical details that a lab that routinely
> conducts FA work on electronic assemblies (there are several who are part
> of Technet) would have a reasonable chance of finding the root cause. At a
> very minimum with the details you have on this issue, the laboratory should
> be able to rule out possible root causes even if they can't find a specific
> root cause. I didn't see any dendritic shorting - is the belief that the
> shorting is internal to the pwb?
>
> Dave Hillman
> Rockwell Collins
> [log in to unmask]
>
>
> On Fri, Apr 8, 2016 at 11:00 AM, Steve Gregory <[log in to unmask]> wrote:
>
>> Good Morning All,
>>
>> We have an assembly that we build here for a customer that we built for
>> some time, over 2,000 assemblies. There have been some failures that our
>> customer has had field returns with that are beginning to escalate. There
>> have been 12 field failures that we know of. The failures are avionic
>> assemblies that have been in the field ranging from 111 days to 472 days.
>> The actual failures are internal +12V to -12V shorts and we need to know
>> why. I have two failed assemblies here. Here are a couple of external
>> photos of a via that shows the short:
>>
>> http://stevezeva.homestead.com/Internal_Short.jpg
>>
>> http://stevezeva.homestead.com/Internal_Short_Close.jpg
>>
>> So my question is, can a lab take these boards and examine them to
>> determine what the root cause actually is from the two assemblies that I
>> have, or does there need to be more samples? What is the range we should
>> expect to pay for this type of analysis?
>>
>> We're trying to work with our PCB vendor on this issue, but I have also
>> been asked by my boss to pursue this with a third party.
>>
>> Thanks!
>>
>> Steve
>>
>>
>> ______________________________________________________________________
>> This email has been scanned by the Symantec Email Security.cloud service.
>> For more information please contact helpdesk at x2960 or [log in to unmask]
>> ______________________________________________________________________
>> --
>>
>>
>> This email and any attachments are only for use by the intended
>> recipient(s) and may contain legally privileged, confidential, proprietary
>> or otherwise private information. Any unauthorized use, reproduction,
>> dissemination, distribution or other disclosure of the contents of this
>> e-mail or its attachments is strictly prohibited. If you have received
>> this
>> email in error, please notify the sender immediately and delete the
>> original.
>>
>
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________
-- 


This email and any attachments are only for use by the intended 
recipient(s) and may contain legally privileged, confidential, proprietary 
or otherwise private information. Any unauthorized use, reproduction, 
dissemination, distribution or other disclosure of the contents of this 
e-mail or its attachments is strictly prohibited. If you have received this 
email in error, please notify the sender immediately and delete the 
original. 

ATOM RSS1 RSS2