TECHNET Archives

April 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Fri, 8 Apr 2016 09:49:24 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ed Hare <[log in to unmask]>
Message-ID:
Subject:
From:
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0 (Mac OS X Mail 9.3 \(3124\))
Parts/Attachments:
text/plain (125 lines)
Hi Steve,

+12V & -12V is 24 volts with a little prepreg layer in between.  Sounds like trouble.

------------------------
Ed Hare
[log in to unmask]




> On Apr 8, 2016, at 9:44 AM, Steve Gregory <[log in to unmask]> wrote:
> 
> Hi again Dave,
> 
> So the PCB is a .090" thick, 8-layer board, the stack-up is this:
> 
> Soldermask
> Layer 1
> ----------
> Ground
> ----------Pre-preg
> Layer 3
> ----------
> +12V
> ----------Pre-preg
> -12V
> ----------
> Layer 6
> ----------Pre-preg
> Ground
> ----------
> Layer 8
> Soldermask
> 
> Steve
> 
> 
> On Fri, Apr 8, 2016 at 10:18 AM, David Hillman <
> [log in to unmask]> wrote:
> 
>> Hi Steve - yes, you have enough physical details that a lab that routinely
>> conducts FA work on electronic assemblies (there are several who are part
>> of Technet) would have a reasonable chance of finding the root cause. At a
>> very minimum with the details you have on this issue, the laboratory should
>> be able to rule out possible root causes even if they can't find a specific
>> root cause. I didn't see any dendritic shorting - is the belief that the
>> shorting is internal to the pwb?
>> 
>> Dave Hillman
>> Rockwell Collins
>> [log in to unmask]
>> 
>> 
>> On Fri, Apr 8, 2016 at 11:00 AM, Steve Gregory <[log in to unmask]> wrote:
>> 
>>> Good Morning All,
>>> 
>>> We have an assembly that we build here for a customer that we built for
>>> some time, over 2,000 assemblies. There have been some failures that our
>>> customer has had field returns with that are beginning to escalate. There
>>> have been 12 field failures that we know of. The failures are avionic
>>> assemblies that have been in the field ranging from 111 days to 472 days.
>>> The actual failures are internal +12V to -12V shorts and we need to know
>>> why. I have two failed assemblies here. Here are a couple of external
>>> photos of a via that shows the short:
>>> 
>>> http://stevezeva.homestead.com/Internal_Short.jpg
>>> 
>>> http://stevezeva.homestead.com/Internal_Short_Close.jpg
>>> 
>>> So my question is, can a lab take these boards and examine them to
>>> determine what the root cause actually is from the two assemblies that I
>>> have, or does there need to be more samples? What is the range we should
>>> expect to pay for this type of analysis?
>>> 
>>> We're trying to work with our PCB vendor on this issue, but I have also
>>> been asked by my boss to pursue this with a third party.
>>> 
>>> Thanks!
>>> 
>>> Steve
>>> 
>>> 
>>> ______________________________________________________________________
>>> This email has been scanned by the Symantec Email Security.cloud service.
>>> For more information please contact helpdesk at x2960 or [log in to unmask]
>>> ______________________________________________________________________
>>> --
>>> 
>>> 
>>> This email and any attachments are only for use by the intended
>>> recipient(s) and may contain legally privileged, confidential, proprietary
>>> or otherwise private information. Any unauthorized use, reproduction,
>>> dissemination, distribution or other disclosure of the contents of this
>>> e-mail or its attachments is strictly prohibited. If you have received
>>> this
>>> email in error, please notify the sender immediately and delete the
>>> original.
>>> 
>> 
>> 
> 
> 
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask] 
> ______________________________________________________________________
> -- 
> 
> 
> This email and any attachments are only for use by the intended 
> recipient(s) and may contain legally privileged, confidential, proprietary 
> or otherwise private information. Any unauthorized use, reproduction, 
> dissemination, distribution or other disclosure of the contents of this 
> e-mail or its attachments is strictly prohibited. If you have received this 
> email in error, please notify the sender immediately and delete the 
> original. 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2