Bob,
Pre-preg I don't know about, but we fill thermal via holes in
conduction-cooled boards using a silver-loaded epoxy. It's part number is
CB-100 from Dupont. Any use?
Pete Duncan
"<Bob
Mcgarry>" To: [log in to unmask]
Sent by: cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
TechNet Subject: [TN] conductive epoxy prepreg
<[log in to unmask]
ORG>
05/30/01
10:58 PM
Please
respond to
"TechNet
E-Mail
Forum.";
Please
respond to
boardguyusa
Does anyone know of a electrically and thermally conductive epoxy prepreg
that can be used to bond PCB's to heatsinks. Material must be conductive
and have the properties of a no-flow type prepreg to avoid flow into gaps
in the heatsink.
Thanks,
__________________________________________________________________
Get your own FREE, personal Netscape Webmail account today at
http://webmail.netscape.com/
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|