In a message dated 05/16/2000 11:08:24 AM US Eastern Standard Time,
[log in to unmask] writes:
> Does anyone have experience with
> polyfunctional FR4 that would care to comment?
>
> Also, would the material designation for the polyfunctional FR4 be "L25",
> even though the Tg is 140 C?
I have found, in general, that bare boards built from a higher Tg material
have a lower propensity towards absorption of HASL fluxes. All other factors
being equal, it makes them a little cleaner, or easier to clean.
Doug Pauls
CSL
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|