We  are considering to install a DMS line instead of electroless copper
plating line.  However some concern has been raised by one of our engineers
that DMS may not be good for high aspect ratio holes.   Therefore I would
like to ask Technetters' opinion on pro and con's of the two different
technologies.

Thanks in advance

M. C. Chu
       
CSS Asia Co., Ltd.
2nd Fl., Myungwoo B/D.
1460-17 Seocho-3-Dong, Seocho-Ku
Seoul, Korea
Tel: 82 2 523 8810   Fax: 82 2 523 1483
[log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2