We are considering to install a DMS line instead of electroless copper plating line. However some concern has been raised by one of our engineers that DMS may not be good for high aspect ratio holes. Therefore I would like to ask Technetters' opinion on pro and con's of the two different technologies. Thanks in advance M. C. Chu CSS Asia Co., Ltd. 2nd Fl., Myungwoo B/D. 1460-17 Seocho-3-Dong, Seocho-Ku Seoul, Korea Tel: 82 2 523 8810 Fax: 82 2 523 1483 [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************