TECHNET Archives

September 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=us-ascii
Sender:
Subject:
From:
Date:
Wed, 17 Sep 2003 09:15:14 -0500
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (61 lines)
Graham,

I looked into this earlier this year.  There are thickness gauges that
measure non-ferrous coatings using eddy-current.  Some have detachable
probes while others have probes integral to the instrument.  The latter is
less expensive and would probably work well if you are measuring coupons.
The ones with detachable probes usually are available in varying probe
sizes.   Depending on what you need, these tools can be quite sophisticated
and also very pricey.  I have contact information on a couple of different
tools,  If you're interested, let me know off line.

-Sue

      ----Original Message----

      Date:    Tue, 16 Sep 2003 15:02:07 -0400
      From:    Collins Graham <[log in to unmask]>
      Subject: measuring the thickness of cured conformal coating

      Hello TechNet!
      I've got a question for the conformal coaters out there.

      Our situation:  We currently measure CCA thickness before
      application, and then again after application & cure of conformal
      coating, to determine how thick a coating we have applied.  We are
      currently using a micrometer to measure the thickness.  Our coating
      thickness is in the 0.001" to 0.005" range.

      My question is: what are others using to do this sort of measurement?
      Are there are better tools out there to do this faster / better?

      Thanks!

      regards,

      Graham Collins
      Process Engineer,
      Northrop Grumman Canada Corporation
      Halifax
      (902) 873-2000 ext 6215


--------------------------------------------------
This message may contain confidential and/or privileged information of
United Technologies Corporation and its affiliated companies.  If you are
not the intended recipient please   1) do not disclose, copy, distribute or
use this information,   2) advise the sender by return e-mail and   3)
delete all copies from your computer.  Your cooperation is greatly
appreciated.
--------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2