We've had good luck with a CMI model CGX-B on dry coating. The unit should
be returned to the factory for recalibration on a yearly basis. I believe it
is an eddy current measurement device and measurements must be made over
copper. I use a half inch square of FR-4 for standardization and
measurement after selective coating and drying. It helps if the design
leaves a small bare copper area in the border. Repeatability is +,- 0.1
mil.
-----Original Message-----
From: Collins Graham [mailto:[log in to unmask]]
Sent: Tuesday, September 16, 2003 3:02 PM
To: [log in to unmask]
Subject: [TN] measuring the thickness of cured conformal coating
Hello TechNet!
I've got a question for the conformal coaters out there.
Our situation: We currently measure CCA thickness before application,
and then again after application & cure of conformal coating, to
determine how thick a coating we have applied. We are currently using a
micrometer to measure the thickness. Our coating thickness is in the
0.001" to 0.005" range.
My question is: what are others using to do this sort of measurement?
Are there are better tools out there to do this faster / better?
Thanks!
regards,
Graham Collins
Process Engineer,
Northrop Grumman Canada Corporation
Halifax
(902) 873-2000 ext 6215
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|