TECHNET Archives

March 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0w6eRa-000BC2C; Mon, 17 Mar 97 09:35 CST
Old-Return-Path:
Date:
Mon, 17 Mar 1997 08:42:55 MST
Precedence:
list
Resent-From:
Message-ID:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11138
TO:
From [log in to unmask] Mon Mar 17 17:
10:52 1997
X-Loop:
Resent-Message-ID:
<"e_Byn.0.91I.zIMBp"@ipc>
X-Juno-Line-Breaks:
2-6,9-11,13-18,20-24
From:
[log in to unmask] (starr devere)
Return-Path:
<TechNet-request>
Subject:
X-Mailer:
Juno 1.15
Resent-Sender:
TechNet-request [log in to unmask]
Parts/Attachments:
text/plain (38 lines)
Looking for options & suggestions regarding how to improve wettability of
Pd-Ag terminated parts using eutectic, water soluable, organic acid
resin, convection reflow  solder process.

Current SMT Process: 
Alpha WS609 solderpaste / conv. reflow / hot DI water wash

I have a board designed with varistors that are supposedly only available
with Palladium-Silver terminations.  The standard process results in
unacceptable yields due to poor wettability.  

Options/Ideas so far:        PROs                    CONs
-------------------------    ---------------------  
----------------------
Change solderpaste alloy     better wetting          extra process
Modify reflow profile        better wetting          none
Different atmosphere         better wetting          extra cost
Solder dip terminations      better wetting          extra cost

Are there any other suggestions or comments about ways to improve
wettability?

Can anyone recommend an inexpensive supplier to solder dip the parts?

Thanks in advance for your comments.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2