Moonman
There's no way a commercial double-sided laminate over 2 mm thick will
use 106 style, or any monofilament cloth. It will be made from 7628 or
7634, with c. 40% - 45% RC. Quite apart from economic factors, the use
of fine cloths with high resin contents will induce slippage, causing
all sorts of dire problems.
Best regards,
Brian
Earl Moon wrote:
>
> Doug,
>
> Very profound and interesting. I'd like to get deeper into this if you will.
>
> The surface layer pregs usually are 106, or so, glass styles. The resin to
> glass ratios are in the 65 to 70% range. I should think this would offset
> any problems suggested.
>
> Just exploring a bit,
>
> Earl
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|