TECHNET Archives

July 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=us-ascii
Sender:
Subject:
From:
Date:
Mon, 15 Jul 2002 08:29:57 +0800
MIME-Version:
1.0
X-To:
Kathy Kuhlow <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (88 lines)
With many QFP's, and other fine-pitch components, there's usually no side
fillet worth speaking of either. The problem with not having a heel fillet
as well really shows up if the board is to be used in a harsh envirnment -
there, the heel fillet is all-important, as it's where the major stresses
are focused. No heel fillet and a measure of vibration, and you'll find
cracks promulgating rapidly through what solder joint you do have, with
obvious consequences.

Replacement pads are not an ideal solution, as they depend on the skill of
the operator to fit them, but the procedure to do so, and the materials
replacement pads are made from, are compliant with IPC-7721 for board
repairs, even class 3's. Circuit Technology Center, Inc do kits of parts
with full procedure manuals.

If you don't do so already, you could bond the affected components to the
board to support them against vibration, adn raise that waiver Kathy
suggested.

Peter



Kathy Kuhlow <[log in to unmask]>    13/07/2002 04:58 AM
Sent by: TechNet <[log in to unmask]>

Please respond to "TechNet E-Mail Forum."; Please respond to Kathy Kuhlow

              To:  [log in to unmask]
              cc:  (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
              Subject: Re: [TN] part/pad mismatch








you might be able to find an after market adapter.  I forwarded your
original post to a company qfp-adapter.com and asked them to help out.

When you mentioned the heel hangs off of the end of the pad, did you mean
that the heel overhangs the front or back of the pad?  If the pad overhangs
the front, well, you are in a pickle.  But if the heel is the only part of
the solder joint that can not be achieved then why not determine the amount
of joint that could be maintained to section 12 and then go for a deviation
from any heel joint requirements due to an incorrect pad layout.

Kathy

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------



<< Attachment Removed : TEXT.htm>>




[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2