TECHNET Archives

July 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=us-ascii
Sender:
Subject:
From:
Date:
Mon, 15 Jul 2002 08:31:25 +0800
MIME-Version:
1.0
X-To:
"D.Terstegge" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (199 lines)
Eccobond 45 is a good adhesive for component bonding when used in harsh
environments.

Peter



"D.Terstegge" <[log in to unmask]>     13/07/2002 05:35 AM
Sent by: TechNet <[log in to unmask]>

Please respond to "TechNet E-Mail Forum."; Please respond to "D.Terstegge"

              To:  [log in to unmask]
              cc:  (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
              Subject: Re: [TN] part/pad mismatch








Hi Graham,

It'll probably be impossible to make this thing look like IPC3, and the
next best thing to worry about is the actual strength of the bonding from
the QFP to the board. I thought that perhaps you can achieve the extra
needed adhesion by using some kind of glue underneath the part (or
embedding it completely). Don't know what kind of adhesive would be best
for the job, but thought I'd propose this alternative kind of solution to
your problem.....

Daan Terstegge
http://www.smtinfo.net

 ----- Original Message -----
 From: Graham Collins
 To: [log in to unmask]
 Sent: Friday, July 12, 2002 8:46 PM
 Subject: Re: [TN] part/pad mismatch

 Hi Steve
 Interesting company!  That said, I don't think I could sell this one to my
 customer - this is a class 3 high rel vehicle electronics beast, and will
 be seeing some serious off-road action.  Their mods might stand up to
 that, but proving it to my satisfaction would be tough, and my customer
 would be more skeptical than I am...  I've also talked with Circuit Tech
 corp about replacing the pads, theoretically possible but again a tough
 sell to the customer.

 If I'm "lucky" this won't be a timing sensitive part, and we will end up
 dead-bugging and wiring the thing.  Ah well, it's only a 72 lead part...

 Thanks!
  - Graham


 regards

 Graham Collins
 Process Engineer,
 Northrop Grumman
 Atlantic Facility of Litton Systems Canada
 (902) 873-2000 ext 6215

 >>> [log in to unmask] 07/12/02 02:52PM >>>
 Hi Graham!

 You're probably gonna have a heck of a time finding some sort of adaptor
 that
 will work, but I have another suggestion.

 Have you ever heard of Additive Services? Go to:

 http://www.additive.com/

 They're a company that has a process to make wireless ECO's, meaning that
 they can add conductors to printed circuit boards to make design changes
 and
 you don't have to add jumper wires.

 I called them and explained your issue. Basically you need some longer
 pads
 so you can get a heel fillet on the device when soldered to the PCB. They
 told me that it would be no problem. However, they can only work with bare
 boards.

 He asked me what the quantity would be, and I told him I didn't know.

 I talked with a gentleman named Darren Cossette at (603) 889-1999, and
 told
 him I would give you the information...

 If this sounds like something that would work, give him a call...

 Hope this helps ;^)

 -Steve Gregory-


 > Good day Technet!  It's Friday and of that I am glad.
 >
 > I have a new design where a part (a quad flatpack, 50 thou pitch part)
 does
 > not match the pads on the board.  As-is, I can attach it but there will
 be
 > no heel fillet as the heel overhangs the end of pad by a fair bit.
 >
 > I have examined and discarded the three obvious options:
 > - re-form the part to fit: not a good option due to the fact that I'd
 have
 > to straighten and then bend the leads in the opposite direction.
 > - buy un-formed parts and form to fit - can do, but schedule will be
 > totally in the dustbin.
 > - re-spin the board to fix the pad layout - again the schedule will be
 > totally out the window.
 >
 > So - that leaves me looking for an adaptor.  Can Technetter's advise me
 of
 > anyone making such beasts on a quick turn basis?
 >
 > As always, thanks.  And a good weekend wish to all.
 >
 > regards
 >
 > Graham Collins
 > Process Engineer,
 > Northrop Grumman
 > Atlantic Facility of Litton Systems Canada
 > (902) 873-2000 ext 6215
 >



 ---------------------------------------------------------------------------------

 Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
 To unsubscribe, send a message to [log in to unmask] with following text in
 the BODY (NOT the subject field): SIGNOFF Technet
 To temporarily halt or (re-start) delivery of Technet send e-mail to
 [log in to unmask]: SET Technet NOMAIL or (MAIL)
 To receive ONE mailing per day of all the posts: send e-mail to
 [log in to unmask]: SET Technet Digest
 Search the archives of previous posts at: http://listserv.ipc.org/archives

 Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
 information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
 ext.5315
 ---------------------------------------------------------------------------------


 ---------------------------------------------------------------------------------

 Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
 To unsubscribe, send a message to [log in to unmask] with following text in
 the BODY (NOT the subject field): SIGNOFF Technet
 To temporarily halt or (re-start) delivery of Technet send e-mail to
 [log in to unmask]: SET Technet NOMAIL or (MAIL)
 To receive ONE mailing per day of all the posts: send e-mail to
 [log in to unmask]: SET Technet Digest
 Search the archives of previous posts at: http://listserv.ipc.org/archives
 Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
 information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
 ext.5315
 ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/html/forum.htm for additional information, or
contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------





[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2