Item Subject: [TN] BGA Assembly
Tom,
In the market, the nozzles for rework stations such as SRT,
Conceptronic and Pace have the same shape as the BGA, namely square.
There is more heat in the four corners than in other location due to
more flow near the corner. When you set the temperature profile, you
may put the thermal couple in the center of BGA. This cause that the
temperature profile at the corner is too high.
The solution may have:
(1)Modify the nozzle---reduce the heat at the corners
(2)Use more thermal couple for setting the temperature profile
(3)If you print the solder paste for rework, stencil aperture at the
corner should be smaller.
(4)If you do not print solder paste for rework, consider the
noe-cleaning tacky flux.
Eden
______________________________ Reply Separator _________________________________
Subject: [TN] BGA Assembly
Author: Non-HP-tomh3 ([log in to unmask]) at HP-Singapore,shargw51
Date: 10/21/98 7:48 AM
I had a lot of 15 boards that I mounted PBGA388 (35mmX35mm), using
Conceptronic BGA rework station. As I was observing the reflow, I
noticed bowing of the plastic laminate on the corners of the component.
Once the component was reflowed, it became level with the PCB, but the
bowing action caused several shorts between the balls under the corners.
Any suggestions on how to correct the problem? The inspection following
the reflow reveal good wetting and reflow on rest of the balls.
Tom Han
Ardent Systems
___________________________________________________________________
You don't need to buy Internet access to use free Internet e-mail.
Get completely free e-mail from Juno at http://www.juno.com
or call Juno at (800) 654-JUNO [654-5866]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|