I had a lot of 15 boards that I mounted PBGA388 (35mmX35mm), using
Conceptronic BGA rework station. As I was observing the reflow, I
noticed bowing of the plastic laminate on the corners of the component.
Once the component was reflowed, it became level with the PCB, but the
bowing action caused several shorts between the balls under the corners.
Any suggestions on how to correct the problem? The inspection following
the reflow reveal good wetting and reflow on rest of the balls.
Tom Han
Ardent Systems
___________________________________________________________________
You don't need to buy Internet access to use free Internet e-mail.
Get completely free e-mail from Juno at http://www.juno.com
or call Juno at (800) 654-JUNO [654-5866]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|