In a message dated 10/11/99 5:43:48 PM Pacific Daylight Time,
[log in to unmask] writes:
<< So it's ammoia , interesting .
What's ammoia's function in temp solder mask ;
if there is nonammoniated version ?
>>
Ammonia, in coatings, is usually present to neutralize the acidity of the
coating, thus rendering it more water soluble. And being volatile, it is
neutralizer that you can cause to go away with heat, thus baking the coating
to a greater level of water resistance.
I suspect strongly that a non-ammoniated version is theoretically possible,
whether it is commercially available, I cannot answer.
Rudy Sedlak
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|