TECHNET Archives

September 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Howard Watson <[log in to unmask]>
Date:
Thu, 27 Sep 2001 10:58:25 -0400
Content-Type:
multipart/alternative; boundary="=_alternative 0051DB8B87256AD4_="
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (2233 bytes) , text/html (3306 bytes)
James,

We do not inspect for solder beads under chip components, and from a
random inspection, I have not seen any.  However, until recently, we have
had a horrendous problem with squeeze out beads, which because of our
no-clean process, have to be picked off one at a time.  I estimate
500,000, give or take 100,000 or so, solder beads per month have been
removed from our boards.

I stated "until recently" we had solder beads, because after changing
solder paste a month ago, the solder beads have virtually gone away, much
to the delight of the operators.  Other process changes like homeplate
aperture design, reduced stencil thickness, and improved reflow profile
have helped a lot, but the new paste put a closure on this issue.  Good
luck!

Howard Watson
Manufacturing Engineer
AMETEK/Dixson




"Marsico, James" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
09/26/01 01:44 PM
Please respond to "TechNet E-Mail Forum."


        To:     [log in to unmask]
        cc:
        Subject:        [TN] SOLDER BEAD SURVEY


Ok... Here we go again.  We are experiencing solder beads found UNDER chip
components.  The following questions are for all SMT assemblers (this info
would be very helpful to me):

1)      Do you look for solder balls under chip devices?
2)      Do you find them?
3)      Do you rework this anomaly?
4)      What workmanship criteria are you working to (i.e. MIL-STD-2000,
IPC-610, other)?

Thanks in advance,
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------




ATOM RSS1 RSS2