TECHNET Archives

June 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Tan Geok Ang <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Tan Geok Ang <[log in to unmask]>
Date:
Tue, 1 Jul 2008 08:24:00 +0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (170 lines)
Hi Ted,
             What is the board thickness of your board design? You might want to increase the board thickness (2mm)...yes stiffener/ solid tray will minimise the issue. 
             Hope things are going well for you.
Regards
GA Tan
(Old Friend)

________________________________

From: TechNet on behalf of Ted Kong
Sent: Tue 7/1/2008 4:59 AM
To: [log in to unmask]
Subject: Re: [TN] Bow PCAs



Hi Ryan,


I did run the board through with the narrower side.  The interesting thing is that the board bowed upward.    When I run the blank boards through twice, I don't see any bowing.  I will consider the stiffeners if I can remove it the bow from other means. 

Thanks for everyone's reply.

Ted


--- On Mon, 6/30/08, Ryan Grant <[log in to unmask]> wrote:

> From: Ryan Grant <[log in to unmask]>
> Subject: Re: [TN] Bow PCAs
> To: [log in to unmask]
> Date: Monday, June 30, 2008, 12:35 PM
> Hi Ted,
>
> The bowing is due to the weight of the heatsink/BGA combo.
>
>
> By 175C, your boards are sure to have reached their glass
> transition
> temperature, which means, even though the board is still a
> solid, it is
> soft and malleable and can easily be distorted.  The weight
> of the
> heatsink/BGA combo is causing the board to sag between the
> oven rails. 
>
> Rotate the board 90 degrees through reflow and the bowing
> should go
> away.  4 inches is usually the minimum conveyor rail width,
> so you are
> in luck, your board will still fit.
>
> If you don't think rotating the board is an option,
> your other
> alternative is Titanium board stiffeners that must be
> attached before
> reflow and removed afterwards.
>
> Thanks,
> Ryan
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Ted
> Kong
> Sent: Monday, June 30, 2008 1:24 PM
> To: [log in to unmask]
> Subject: [TN] Bow PCAs
>
> Hi Technetters,
>
> I have a 14.5" x 4" PCB that bows after top side
> reflow.  I haven't
> measure the actural bow amount yet, but it looks like it
> will meet IPC
> spec.  However, I want to see what I can do to eliminate
> it. 
>
> I run a blank board through the same reflow profile and
> don't see any
> bowing.  The production boards do not have any bowing after
> bottom side
> reflow.  Bowing only occur after the top side reflow.  I
> believe the
> bowing is due to the two 40mm2 BGAs on the board, which is
> located 4"
> from the long edge (center from the narrow width).  Both
> BGAs have large
> heat-sinks attached to them.  I reflowed three additional
> boards on a 10
> zone reflow oven (instead of a 7 zone) oven, but didn't
> see any
> improvements.  Can anyone give me any other suggestion on
> how to
> eliminate the bowing?  Is my assumption of the cause
> correct?
>
> Thanks all in advance.
>
>
> Ted
>
>
>      
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using
> LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with
> following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send
> e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send
> e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using
> LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with
> following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send
> e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send
> e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------


     

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2