     Hi Mike -
     
     Take a look at ANSIJ-STD-003 Solderability Tests For Printed Wiring 
     Boards. The specification contains several methods for testing of 
     printed wiring boards.
     
     
     Dave Hillman
     JSTD 003 CoChairman
     Rockwell Collins


______________________________ Reply Separator _________________________________
Subject: Solderability Tests for PCBs
Author:  [log in to unmask] at ccmgw1
Date:    7/30/97 1:34 PM


     
Good Morning,
     
I am in need of implementing a solderability test for PCBs received from 
bareboard suppliers.  The test should be simple and quick.  Does anyone know of 
a procedure for solderability that might be used?
     
mike
     
     
-- 
    /\    
   _\/_   
  /_/\_\  
     
Mike Masters
QA Materials Engineering Section
Office: (919) 479-3771
FAX:    (919) 479-3328
Internet:  [log in to unmask]
     
     
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2