Hi Mike - Take a look at ANSIJ-STD-003 Solderability Tests For Printed Wiring Boards. The specification contains several methods for testing of printed wiring boards. Dave Hillman JSTD 003 CoChairman Rockwell Collins ______________________________ Reply Separator _________________________________ Subject: Solderability Tests for PCBs Author: [log in to unmask] at ccmgw1 Date: 7/30/97 1:34 PM Good Morning, I am in need of implementing a solderability test for PCBs received from bareboard suppliers. The test should be simple and quick. Does anyone know of a procedure for solderability that might be used? mike -- /\ _\/_ /_/\_\ Mike Masters QA Materials Engineering Section Office: (919) 479-3771 FAX: (919) 479-3328 Internet: [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************