TECHNET Archives

August 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Black, Paul" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 22 Aug 2003 08:10:14 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (45 lines)
Thanks for the advice, Werner. I didn't realize this document existed. The
original recipe was determined by running a thermocoupled assembly through
the oven and matching the time/temperature graph supplied by the paste
manufacturer. When the manufacturer made adjustments to the recipe, it was
done with the aid of a Super MOLE.

Thank you,
Paul Black
Manufacturing Engineer
Kronos



-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Friday, August 22, 2003 7:49 AM
To: [log in to unmask]; [log in to unmask]
Subject: Re: [TN] Soft solder


Hi Paul,
Are you profiling your assemblies to determine a proper oven recipe? Look ay

IPC-7530.
Just calling in your paste supplier is in many cases not sufficient.

Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL  32174  USA
Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2