I'm seeking input/confirmation about a problem I am observing for no
clean wave soldering process. The problem is a constant build-up of
white powdery flux residue in/around flux spray system. Our wave
operators remove the residue around spray nozzle every 2/4 hours with
brush/alcohol. It gets build-up quickly around the whole spray flux
system.

Boards that are wave processed have invisible white residue. It
requires a clean wipe to see some. This flux is alcohol-based no clean
with 2% resin as solid content. I am used to using alcohol-based no
clean with organic chemistry as flux activator and didn't have any issue
with white flux residue build-up.

J-STD-004 calls out four classifications of flux composition
(Rosin/Resin/Organic/Inorganic). Is white powdery residue build-up from
resin formulation in the flux we are using?

any thoughts?
thanks


Matthew S. Park
Preco Electronics
tel: (309)-263-7788
fax: (309)-266-6674
1651 N. Main Morton. IL 61550

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2