mmm there's a thought... but suggest also plenty of rinsing as well though
after to remove neutral salts,
also make sure neat chemicals don't "see" each other direct.
A friend of mine used to put bits of copper in his iron pickling bath, he
didn't know why but just did because he was told to by an old-time expert
and so on back. It's sort of sense as amongst other things the copper would
plate out on the iron and passivate it I suppose, and this is not too far in
concept from the old time "killed spirits" fluxes (where Zinc is added).

Best regards

Mike



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of <Rudy Sedlak>
Sent: Tuesday, December 04, 2001 1:24 PM
To: [log in to unmask]
Subject: Re: [TN] Rust Removal


Earl, the bad news is that when you have rust, the surface has been
seriously
activated, and virtually any chemistry that removes rust easily will leave a
surface that re-rusts very rapidly.

Hydrochloric Acid is likely the fastest, easiest way to get rust off a
surface, and the easiest way to get fairly concentrated Hydrochloric Acid is
to buy a bottle of toilet cleaner, most liquid toilet cleaners are pretty
concentrated HCl.  The best way to prevent rust from re-occurring is
neutralize the acid as soon as the rust is removed, and for a cheep and easy
way to do that, use a diluted laundry detergent.

This will still leave a surface that re-rusts faster than the original
rusted, however, short of coating the surface with an organic coating, it is
the best/easiest approach.

Good luck

Rudy Sedlak

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2