Thermount is duPonts name for it's random Aramid fiber.  It is used to make 
boards where expansion in x and y are constrained.  There are several 
suppliers of laminate based on it that I am aware of Neltec for epoxy based, 
and Arlon for polyimide based.
     DuPont contacts are:  David Powell 207-865-4090
[log in to unmask]

     or Bill Allfather at 302-999-2250

     Arlon is at 909-987-9533

     Neltec is at 602-967-5600

 ----------
From: [log in to unmask]
To: [log in to unmask]
Subject: Fab - material
Date: Friday, April 18, 1997 10:10AM

     Could someone point me in the right direction to get
     information on Thermount material.
        Thankyou
        Don Bloye
     PC World
        [log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2