TECHNET Archives

October 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Mon, 5 Oct 1998 22:16:48 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
Roger Mouton <[log in to unmask]>
Content-transfer-encoding:
7bit
Parts/Attachments:
text/plain (30 lines)
Jacob -

The term throwing power is often misused.  It refers to the uniformity of a
deposit thickness over a varying current density range.  It's often confused
with the cosmetic uniformity achieved when the deposit "looks" the same in the
high and low current density areas of a cathode.

Good throwing power would thus be achieved when the deposit on a circuit board
is 1 mil in the hole and 1 mil on the surface.....everywhere on the board.
Or, 1 mil on the surface and 1 mil in the bottom of a blind via hole,
especially a deep one.  That's good throwing power.  Thought of another way:
uniform plating thickness distribution in any cavity or blind area where there
is a disparity of current distribution from high to low current density areas.
Stay put and see what else shows up on this question.  It can elicit a
multitude of responses.

Roger Mouton

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2