Ann,
Why do you believe it's a typo? 6-12 microns of Ni is a lot (more than
needed), but certainly possible. And so is 2-4 microns of Au. You may be
thinking they want 6-12 and 2-4 microinches. That would be immersion gold
range. Nobody can put on 2-4 microns of gold by immersion process. Further,
I don't think there are immersion hard gold baths. So it's got to be
electrolytic. If it is a touch pad, thick hard gold makes sense. I can give
a few supplier names off the Technet if you like.
Timothy Reeves
ECD Circuit Board Division
13626 South Freeman Road
Mulino, OR 97042
[log in to unmask]
(503) 829-9108 (800) 228-8198 FAX (503) 829-5482
> ----------
> From: Anne Ledger
> Sent: Tuesday, February 15, 2000 12:13
> Subject: Hard gold question
>
> Good afternoon Technet,
>
> We are looking for a referral for a customer that requires the
> following:
>
> Gold plate on top side only (selective)
> Gold plate over Nickel Plate 6-12 microns (must be a typo)
> Gold plate thickness 2-4 microns (appears to be immersion)
> Gold plate hardness 130-200 (knoop scale)
>
> This is a little 4 layer, 1 oz copper all thru. It looks like a touch
> keypad.
> Anyone know where to get this one made?
>
> Thanks in advance for any input, we'll forward on all names to the end
> user.
>
> Anne Ledger
> EMDS, Inc.
> [log in to unmask]
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|