TECHNET Archives

September 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
"<Jason M. Smith>" <[log in to unmask]>
Date:
Mon, 14 Sep 1998 08:23:50 -0400
Content-Type:
text/plain; charset=us-ascii
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (24 lines)
My first stab at your situation would be that you're not getting a good time
above reflow to allow your intermetallic layer to form a good bond between your
solder and lead.  The intermetallic layer is hard and brittle, and should be
minimized, however it is necessary.  Do a cross section of the bond if you're
even getting good wetting and wicking to the lead.  Analysis under a scope is
probably going to answer your own question.  Appears that you either have too
much or not enough heat.  Your profile is the key in my opinion.

Jason Smith
Process Materials Engineer
Lexmark Electronics

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2