TECHNET Archives

August 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Bartkowaik Christine <[log in to unmask]>
Date:
Tue, 21 Aug 2001 15:34:39 -0400
Content-Type:
text/plain
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (71 lines)
Jorge:

This can be caused by:
a)      Too slow a ramp rate.
b)      Excessive paste deposit during printing.

Chris

        -----Original Message-----
        From:   Jorge Rodriguez [SMTP:[log in to unmask]]
        Sent:   Tuesday, August 21, 2001 2:57 PM
        To:     [log in to unmask]
        Subject:        [TN] Solder Beads (not solder balls)

        Fellow technetters,

        We are having tons of issues with solder beading, even on boards
were we
        didn't have the issue before. We're clueless, we suspect of the
solder paste
        (63-37 Water Soluble), it looks slumpy amd watery, but we're not
sure. I
        know solder beading can be solved by designing the stencils with
home-base
        aperture, but what we're seeing here is across the board, not just
one
        particular assembly but several. Does anyone have experience dealing
with an
        issue like this?, could solder beading caused by the oven profile or
is it
        more like solder paste related?


        Any comments would be appreciated.


        Jorge Rodriguez
        Process Engineer
        Varian Electronics Manufacturing
        E-mail: [log in to unmask]


----------------------------------------------------------------------------
-----
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
        Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315

----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2