TECHNET Archives

March 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 1 Mar 2006 08:33:14 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Eddie Rocha <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
8bit
Content-Type:
text/plain; charset="ISO-8859-1"
From:
Eddie Rocha <[log in to unmask]>
Parts/Attachments:
text/plain (31 lines)
I have some questions regarding immersion silver. IPC-4553
standard refers to a thin and thick deposit silver as if
there are two different type of silver formulations. I've
spoken to multiple domestic chemical suppliers of the
silver process and they all offer the thick deposit
version. One supplier stated that they can provide a thin
deposit with their thick deposit version with no
solderability issues. The IPC standard states not to do
this.

Question 1: Why can't a thick deposit silver version be
used to deposit a thin deposit (3-5 uin)?

Question 2: Who supplies a thin deposit silver?

Question 3: Would the thin silver deposit perform better
than a thick deposit silver when press fitting pins?

Thank you,
Eddie Rocha

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2